Chapter 6

Powder metallurgy

Powder metallurgy starts with particles and develops a useful part through shaping and bonding. Unlike dense-metal forming, compaction changes bulk volume by reducing pores. Porosity may be a defect to eliminate or a useful designed feature.

6.1 Powder production and characterisation

Past papers · ME 2020–2026 (10 papers): 1 question, 1 mark

RouteMechanism and typical powder characteristic
AtomisationLiquid broken into droplets; gas atomisation commonly gives rounded particles; water atomisation often more irregular
Mechanical comminutionCrushing/milling breaks brittle feed or repeatedly deforms and fractures it; irregular shape, possible contamination
Chemical reductionOxide reduced to metal; porous/spongy particles may result
Electrolytic productionMetal deposited electrolytically, then collected and processed; often dendritic
Carbonyl decompositionVolatile carbonyl decomposed to fine metal powder for suitable metals

Particle size distribution is measured by sieving for suitable coarse powders, laser scattering/diffraction or other appropriate methods. Laser scattering infers size from the scattering pattern; it is not simply a reflectivity test. Shape, surface oxide, apparent density, flowability and compressibility also affect die filling and bonding. Fine particles have high specific surface but may flow poorly and oxidise readily; a suitable size distribution can improve packing.

6.2 Compaction and sintering

Blend/mix powders and additives, compact a green part, remove lubricant/binder as required, sinter in a controlled atmosphere, then finish. Blending can combine size fractions of one powder; mixing combines constituents. Green strength comes from particle contacts/interlocking and binders before full sintered bonding.

Uniaxial die pressing suits repeatable shapes ejectable along the pressing direction. Die-wall friction causes pressure and density gradients; double-action pressing can reduce them. Cold isostatic pressing applies fluid pressure through a flexible mould; hot isostatic pressing combines pressure and temperature. Metal injection moulding uses a powder–binder feedstock, then debinding and sintering; it is not injection of bulk molten metal.

Sintering forms bonds/necks and may densify the compact. The driving force is reduction of surface energy; diffusion and other transport mechanisms act at elevated temperature. Solid-state sintering remains below the solidus of the constituents involved. In liquid-phase sintering, a fraction melts while a solid skeleton remains. Neck growth does not automatically imply full densification; surface diffusion alone can grow necks without bringing particle centres closer.

6.3 Secondary operations and applications

OperationPurpose
Sizing / repressing / coiningImprove dimensions, densify locally or add detail
ImpregnationFill connected pores with oil or resin; self-lubrication or sealing
InfiltrationFill connected pores with a lower-melting liquid metal; increase density/strength or seal
Powder forgingFurther densify and shape a prepared powder preform
Heat treatment / machining / finishingAdjust properties and critical dimensions where required

Applications include self-lubricating bearings, porous filters, small gears, cemented-carbide tools, electrical contacts and refractory-metal parts. Powder routes allow compositions and porosity difficult to obtain by ordinary casting. High material utilisation and repeat production are advantages; powder cost, tooling cost, density gradients, residual pores and ejection restrictions are limitations. A conventional sintered part need not have the fatigue strength or ductility of its fully dense wrought counterpart.

Last-minute recall

  • Powder shape and distribution matter as much as nominal size.
  • Laser scattering can determine particle size distribution.
  • Compaction reduces pores; green strength precedes sintering.
  • Sintering does not require complete melting.
  • Impregnation uses oil/resin; infiltration uses molten metal.
  • Density-based shrinkage needs mass conservation.
  • Porosity enables filters and oil-retaining bearings but can reduce structural properties.

Revise offline: the whole Manufacturing Processes handbook as one PDF

51 pages · 2.0 MBFree to read online. Sign in to download the PDF.We save the handbook, version and request time in My downloads. Privacy policy

All chapters · Corrections