Design basis and material models
A design calculation pairs a load level with a compatible resistance model. Working loads belong with permissible stresses; factored actions belong with design strengths. Concrete and reinforcing steel have different safety factors.
1.1 Working stress, ultimate load and limit states
Past papers · CE 2020–2026 (14 papers): 1 question, 1 mark
Working stress design checks elastic stresses under service loads against permissible values. Its safety margin is mainly built into the allowable stresses. Ultimate-load design checks collapse under enhanced loads but, alone, does not establish acceptable deflection or cracking. Limit-state design checks both strength and serviceability, with separate factors for actions and resistance.
A characteristic material strength has at most 5% of results below it. A characteristic load has a 95% probability of not being exceeded during the structure's life. Safety against collapse does not imply fitness for use: cracking, deflection and vibration can govern first.
1.2 Concrete and reinforcement properties
Past papers · CE 2020–2026 (14 papers): 1 question, 1 mark
is the characteristic compressive strength of a 150 mm concrete cube at 28 days, in MPa. Thus M25 means a 5-percentile cube strength of 25 MPa, not a mean strength of 25 MPa. is reinforcement characteristic yield strength or 0.2% proof stress (MPa).
| Age at loading | 7 days | 28 days | 1 year |
|---|---|---|---|
| Default | 2.2 | 1.6 | 1.1 |
The concrete thermal coefficient depends on aggregate; IS 456 gives a range of to /K. Use the specified value. Detailed cement, aggregate, mix-design and testing procedures belong to the Construction Materials and Management handbook.
1.3 Load combinations and code factors
Past papers · CE 2020–2026 (14 papers): 1 question, 2 marks
Use DL for dead load, IL for imposed load, and WL for wind load; substitute earthquake load EL for WL. Include member self-weight before factoring. Use both signs of the lateral action where relevant; do not combine peak wind and earthquake as simultaneous events.
For linear analysis, factor the characteristic actions before solving or factor their separate effects afterwards. With nonlinear response, those operations need not commute.
1.4 Removed topic: prestressed beams
Prestressed concrete beams are not in the GATE 2027 CE syllabus. Past questions on prestress, tendon profiles or prestress losses are not counted in this handbook.
Last-minute recall
- Characteristic concrete strength is a cube-strength fractile.
- WSM uses service actions; LSM collapse uses factored actions.
- Reinforcing steel: ; structural steel yielding: .
- already includes the reinforcement safety factor.
- Add self-weight before applying load factors.
- Creep depends on sustained stress and loading age; shrinkage need not require load.