Chapter 1

Mechanical properties and material tests

Separate stiffness, strength and energy absorption before comparing materials. A test result belongs to its specimen geometry, temperature and loading rate; hardness and impact values are not universal strength measures.

1.1 Property vocabulary and ductility

PropertyMeaning for selectionCommon confusion
ElasticityRecovery of deformation after unloadingA low modulus does not imply poor elastic recovery
PlasticityPermanent deformation without immediate fractureIncludes forming behaviour, not only tensile elongation
StiffnessResistance to elastic deformation; material measure EEA component's stiffness also depends on geometry
StrengthStress associated with yielding or failureSpecify yield, ultimate tensile or compressive strength
DuctilityPlastic deformation available before fracture in tensionMalleability concerns plastic deformation under compression
BrittlenessFracture with little macroscopic plastic deformationA brittle material may have high compressive strength
ResilienceRecoverable elastic energy per volumeToughness includes deformation up to fracture
HardnessResistance measured by indentation, scratch or rebound testHardness scale and test conditions are essential

Here EE is Young's modulus in Pa. Yield strength SyS_y and ultimate tensile strength SuS_u are positive stress magnitudes in Pa. For a material without a clear yield point, a specified proof stress is used; 0.2% proof stress corresponds to a permanent strain of 0.002. Carbon and nitrogen pinning of dislocations helps explain the upper/lower yield-point phenomenon in mild steel. Plastic prestraining can increase subsequent forward yield strength and reduce reverse yield strength (Bauschinger effect).

1.2 Resilience and toughness

Toughness requires both stress capacity and deformation capacity. A strong but very brittle material can absorb less energy than a weaker ductile one. Modulus of toughness is an energy density, not an elastic modulus.

1.3 Indentation hardness

Brinell measures a spherical impression; Vickers measures diamond-pyramid diagonals; Rockwell measures a permanent depth increment. The specimen must be thick enough and indents sufficiently separated to avoid support and edge effects. Use the test scale given; conversions between scales and strength are empirical and material dependent.

TestIndenter/readoutUseful application
BrinellCarbide ball; optical impression diameterBulk hardness of metals with relatively coarse microstructure
VickersSquare diamond pyramid; mean diagonalBroad hardness range; small loads for individual phases/cases
KnoopElongated diamond impression; long diagonalMicrohardness of thin layers or brittle materials
Rockwell BBall; permanent depth incrementRelatively soft metals
Rockwell CDiamond cone; permanent depth incrementHardened steels
Shore reboundRebound heightComparative dynamic hardness

1.4 Impact strength and transition behaviour

Charpy uses a horizontally supported notched specimen struck opposite the notch. Izod uses a vertical cantilever specimen struck on the notched side. Absorbed energy depends strongly on notch geometry and test temperature; the two tests are not interchangeable.

BCC ferritic steels commonly show a ductile-to-brittle transition on cooling. A lower temperature, sharper notch, higher loading rate and greater constraint can favour brittle fracture. FCC metals generally do not show the same sharp transition. A transition temperature needs a criterion, such as a stated absorbed energy or fracture appearance.

1.5 Time, temperature and loading rate

Creep is time-dependent deformation under sustained stress. It becomes particularly important for metals at a substantial fraction of absolute melting temperature; polymers can creep at room temperature. There is no universal onset temperature.

Creep stageStrain-rate trendPhysical interpretation
PrimaryDecreasesHardening initially dominates recovery
SecondaryApproximately constant and minimumCompeting processes reach a near balance
TertiaryIncreases towards ruptureDamage, cavitation and/or reduction of load-carrying area

At constant load, necking raises true stress and can accelerate tertiary creep. Higher temperature or stress usually increases creep rate and shortens life. Finer grains can improve ordinary yield strength yet worsen grain-boundary-controlled creep; coarse-grained or single-crystal hot-section alloys exploit this distinction. Increasing strain rate usually raises metallic flow stress and can reduce ductility, but trends depend on material and temperature. Fatigue is progressive damage under cyclic loading, even below static yield; see Machine Design for life equations.

Last-minute recall

  • Stiffness, strength, hardness and toughness answer different questions.
  • Ductility percentages use original length or area as denominator.
  • Resilience uses elastic area; toughness extends to fracture.
  • Brinell and Vickers formulas here require kgf and mm.
  • Rockwell reads depth, not impression diameter.
  • Impact energy is not a stress and is not fracture toughness.
  • Creep is time dependent; fatigue requires cyclic loading.

Revise offline: the whole Engineering Materials handbook as one PDF

40 pages · 1.7 MBFree to read online. Sign in to download the PDF.We save the handbook, version and request time in My downloads. Privacy policy

All chapters · Corrections