MOS capacitor
The gate voltage divides between oxide voltage and semiconductor surface potential. Work-function difference and oxide charge shift the reference voltage. Establish substrate type and voltage signs before reading a capacitance curve or calculating threshold.
6.1 Flat-band voltage and gate-charge balance
Past papers · EC 2020–2026 (7 papers): 1 question, 2 marks
Start with a p-type substrate, gate voltage relative to bulk, and surface potential . Positive bends electron band energies downward. Primes denote capacitance or charge per unit area.
An ideal MOS capacitor has matched work functions and no oxide/interface charge, hence . A nonzero work-function difference alone shifts flat band even in a perfect insulating oxide. Negligible gate leakage does not imply zero gate charge.
6.2 Accumulation, depletion and inversion
Let for a fully ionised p-type bulk with . It is a positive magnitude, although in that bulk.
| p-substrate condition | Surface potential | Surface behaviour |
|---|---|---|
| Accumulation | More holes than in bulk; semiconductor charge positive | |
| Flat band | No band bending; net semiconductor charge zero | |
| Depletion | Holes removed; exposed acceptor ions negative | |
| Surface intrinsic | ||
| Weak inversion | Electrons exceed holes at surface but remain below bulk majority density | |
| Conventional strong-inversion threshold |
For an n substrate reverse gate and surface-potential polarities and interchange carrier types. Relative to flat band, a positive gate accumulates electrons on an n substrate and a negative gate drives it towards hole inversion.
6.3 Threshold and inversion charge
Past papers · EC 2020–2026 (7 papers): 3 questions, 4 marks
The threshold condition is a surface-density criterion. Gate work function and oxide charge can make an n-channel threshold negative even with a p-type substrate; substrate type alone does not set the threshold's sign.
6.4 MOS capacitance versus gate voltage
The measured small-signal capacitance depends on whether minority inversion carriers can respond during the AC cycle, and on whether the DC bias had time to establish inversion. Specify both time scales.
| Region/measurement | Measured capacitance |
|---|---|
| Strong accumulation | Approaches at low and high frequency |
| Depletion | Falls as increases; oxide and depletion capacitances in series |
| Strong inversion, quasistatic/low frequency | Returns towards as inversion charge follows |
| Strong inversion, high AC frequency but equilibrated DC bias | Stays near ; minority charge cannot follow AC |
| Rapid DC sweep without enough minority generation | Deep depletion: and capacitance below the usual minimum |
Qualitative p-substrate MOS capacitance curves; flat band and threshold refer to the marked gate voltages.
Interface traps that exchange charge with the semiconductor can stretch and frequency-disperse the curve. Fixed oxide charge primarily shifts it horizontally. Do not treat deep depletion as the equilibrium high-frequency curve.
Last-minute recall
- Distinguish per area from total .
- Positive oxide charge makes flat-band voltage more negative.
- Positive surface potential bends electron energies downward.
- On p material, threshold is conventionally .
- The gate must supply both depletion charge and inversion charge.
- High-frequency inversion capacitance differs from quasistatic inversion capacitance.
- Deep depletion requires inadequate minority-carrier supply during the bias change.